In order to decrease Reducing Agent Rate (RAR) and CO2 emission of blast furnaces, it is important to decrease slag volume. In NSSMC, more than 70% of blast furnace burden is sinter ore, so slag volume control is very important. However slag contents of sinter feeds are increasing because of resource deterioration. Therefore, using high amount of iron ore concentrate, which has relatively lower slag contents, is desired. Nevertheless, it causes decreasing of the permeability of the sintering bed and sinter productivity.
In order to increase the amount of concentrate, NSSMC has developed the new technique adding micro-particles for binder. In this report, vertical wet ball mill was installed on sub granulation line of Wakayama No.5 sinter plant. In this line, about 0.4% of Australian pisolite ore was ground to -10 micron > 60% and added into intensive mixer with iron concentrate and other sinter feeds. After mixing, they were granulated by a pan-pelletizer. After that, they were charged into sinter machine with other materials granulated in main granulation line with two drum mixers. It was confirmed that up to 13.5wt% of concentrate can be used without decreasing of sinter productivity by adding micro-particles.
Author
Mr
Yasuhide Yamaguchi
(Nippon Steel & Sumitomo Metal Corporation)
Co-authors
Dr
Chikashi Kamijo
(Nippon Steel & Sumitomo Metal Corporation)
Mr
Hironari Umemoto
(Nippon Steel & Sumitomo Metal Corporation)
Dr
Kenichi Higuchi
(Nippon Steel & Sumitomo Metal Corporation)
Mr
Masaki Hara
(Nippon Steel & Sumikin Koutetsu Wakayama)
Dr
Masaru Matsumura
(Nippon Steel & Sumitomo Metal Corporation)
Dr
Seiji Nomura
(Nippon Steel & Sumitomo Metal Corporation)