26–29 Jun 2017
Austria Center Vienna
Europe/Vienna timezone

Retention characteristics of ultra-low carbon steel slab corner shape and its influence on edge defects of steel strip

28 Jun 2017, 09:30
20m
Room M (Austria Center Vienna)

Room M

Austria Center Vienna

Bruno-Kreisky-Platz 1 1020 ViennaAustria
Oral Presentation New developments in casting technologies Surface defects in slab casting

Speakers

Mr Hui Zhang (Central Iron and Steel Research Institute)Mr Minglin Wang (Central Iron and Steel Research Institute)

Description

Based on the numerical simulation and industrial experiment research, the retention characteristics of the ultra-low carbon steel slab corner shape in the hot rolling process and its influence on the edge defects are analyzed. Numerical calculation results show that, the chamfered face changes to be circle arc during hot rolling process. The uniformity of stress distribution is improved. The deformation of corners is more stable. That is benefit for controlling edge seam defect. The industrial test results show that chamfered shape can be maintained to the end of rough rolling with the small width reduction. Corner temperature is higher and uniform in rough rolling process. The chamfered shape is also retained after rough rolling, and that is benefit for stable deformation during finish rolling. Thereby the edge seam defect will be eliminated and the possibility of the occurrence of the defect on surface is reduced radically. The statistical results of industrial rolling show that the edge seam defect is effectively controlled by using chamfered slab.

Author

Mr Hui Zhang (Central Iron and Steel Research Institute)

Co-authors

Mr Minglin Wang (Central Iron and Steel Research Institute) Mr Peng Hu (Central Iron and Steel Research Institute)