EFFECT OF COOLING RATE ON THE POROSITY DEFECT IN THE THICK ALUMINUM CASTING BY 3D COMPUTED TOMOGRAPHY ANALYSIS

20 Jun 2019, 16:50
20m
Auersperg 2 (IMLAUER HOTEL PITTER SALZBURG)

Auersperg 2

IMLAUER HOTEL PITTER SALZBURG

Rainerstraße 6, 5020 Salzburg, Austria
Oral Presentation Solidification processing

Speaker

In-Sung Cho (Korea Instititue of Industrial Technology)

Description

In the present study, effect of cooling rate on the formation of the porosity in the thick aluminum sand casting was investigated. Nowadays large scale thick aluminum casting replaces steel frame for vacuum chamber for semiconductor production, with the consideration of weight and cost reduction. Several thick aluminum castings were manufactured using chill with temperature measurements. The castings were inspected by using 3D computed tomography in order to quantify the porosity defect density in the castings. Effect of the thickness of the chill on the porosity defect density were discussed.
Speaker Country South Korea

Author

In-Sung Cho (Korea Instititue of Industrial Technology)

Co-authors

Mr Hee-Kwon Lee (Daeshin Metals, Co. Ltd.) Dr Seung-Mok Yoo (Korea Institute of Industrial Technology) Dr Si-Young Kwak (Korea Institute of industrial Technology) Mr Yong-Hyun Kim (Daeshin Metals, Co. Ltd.)

Presentation materials